Abstract

The results of hydrogen sorption and desorption processes investigation at commercially pure titanium alloy during hydrogenation at gas atmosphere are shown in this article. Titanium alloy hydrogenation at temperatures 350, 450 и 550 °С leads to δ-hydrides formation in samples’ volume. Hydrogen sorption rates were calculated on the linear parts of sorption curves and equal to 0.15·10-4 wt%/s at 350 °C, 0.86·10-4 wt%/s at 450 °C, 1.55·10-4 wt%/s at 550 °C. Phase transition in titanium-hydrogen system during thermally stimulated hydrogen desorption investigation by the means of short-wave diffraction of synchrotron radiation shows hydrides dissociation until 520-530 °C. Then α→β transition takes place until 690-720 °C and at this temperatures the phase transformation ends and additional hydrogen desorption peak appears in thermally stimulated hydrogen desorption curve. Defect structure at different hydrogen concentration investigation by the means of electron-positron annihilation techniques shows that hydrogen penetration into titanium leads to crystal lattice expansion. It initiates vacancy-type defects formation which reacts with hydrogen and forms defect-hydrogen complexes.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.