To promote a better understanding of failure behavior of high burnup PWR fuel rods during reactivity initiated accidents (RIAs), tube burst tests have been performed with artificially hydrided Zircaloy-4 specimens at room temperature and at 620 K. Pressurization rate was increased to a maximum of 3.4 GPa/s in order to simulate rapid pellet/cladding mechanical interaction (PCMI) that occurs in high burnup fuel rods during a pulse-irradiation in the Nuclear Safety Research Reactor (NSRR). Hydrogen content in the specimens ranged from 150 to 1,050 ppm. Hydrides were accumulated in the cladding periphery and formed ‘hydride rim’ (radially-localized hydride layer) as observed in high burnup PWR fuel claddings. The hydrided cladding tubes failed with an axial crack at the room temperature tests. Brittle fracture appeared in the hydride rim, and failure morphology was similar to that observed in the NSRR experiments. The hydrides rim obviously reduced burst pressure and residual hoop strain at the tests. The residual hoop strain was very small even at 620K when thickness of the hydride rim exceeded 18% of cladding thickness. The present result accordingly indicates an important role of the hydrides layer in high burnup fuel rod failure under RIA conditions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.