Abstract

Nomex honeycomb composite (NHC) has been increasingly used in the automotive, aerospace and defence applications due to its excellent thermal and mechanical properties. Its complex cellular hexagonal thin-walled configuration, heterogeneous, soft and brittle nature pose substantial processing defects such as burr formation, tearing of walls, surface roughness, dimensional inaccuracy and low machining quality during conventional machining (CM). These surface defects have a substantial influence on the operating life and functional performance of its sandwiched structural members. Hybrid ultrasonic vibration assisted machining (HUSVAM) technology has been introduced to overcome such limitations. For an in depth research on HUSVAM of NHC using ultrasonic toothed disc cutter (UTDC), three dimensional finite element model was developed and experimental validation was carried out. Numerical simulation and experimental results were found to be in good agreement with one another. The influence of various machining parameters including ultrasonic tool vibration amplitude (UTVA), feed rate (FR), depth of cut (DoC) and spindle angular speed (SAS) on NHC cutting forces, chip formation and surface quality was investigated using both HUSVAM and CM techniques. Furthermore, stresses, deformation and forces near tool-workpiece interaction along with the surface topography and morphologies were also analyzed and compared for various operating conditions. A reduction in the cutting forces was found with the increase of SAS and UTVA (up to 65.47 % and 65.74 %, respectively). Although, the cutting forces were observed to increase by increasing the DoC and FR (up to 159.45 % and 126.33 %, respectively). DoC has greater impact on the cutting forces among all machining parameters according to 4 levels, 4 factors (L16) orthogonal experiments based on Taguchi method. The results show that chip formation and machining quality of NHC can be improved with HUSVAM technique using UTDC. HUSVAM also reduced the cutting forces (up to 73 %) compared to CM. Ultrasonic toothed disc cutter generated large number of burr with very short length, no tearing defects and no uncut fibers as observed from scanning electron microscopy of NHC hexagonal cell structure, walls and triple points. A burr formation of 10 % was realized during HUSVAM of NHC cores for Fx≤3N, while it was found up to 20 % if Fx>3N, compared to at least 40 % during CM. The finite element model developed can be used to investigate the influence of HUSVAM on modern difficult to machine materials for enhanced surface quality.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call