Abstract
The effects of simultaneous use of recycled aggregates and ground blast furnace slag as a percentage of cement-constituting materials on different properties of fresh self-compacting concrete (SCC) are investigated in this study. To this end, three series of SCC mixtures with a fixed volume of cement paste equalling 380 ltr/m3 (2.36 gal/ft3) and the replacement ratio of coarse aggregates (fifty percent and one hundred percent) and total aggregates (zero percent, fifty percent and one hundred percent) were prepared. The water content ratios in the first, second and third series were 0.4, 0.45, and 0.5, respectively. The results of the compressive strength tests for 7-day, 14-day and 28-day cubic specimens and compressive strength and Brazilian test results for 28-day cylindrical specimens were used as control parameters governing the SCC resistive quality. The results of fresh SCC tests (including slump-flow and T50 tests, V-funnel test, and L-box test) showed that the negative effect of recycled fine aggregates on fresh SCC properties is significantly more than that of recycled coarse aggregate. However, recycled SCC with acceptable properties can be obtained with a slight increase in the amount of superplasticisers used in the presence of slag.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.