The powder compact was directly sintered by a pack boriding process to prepare a Fe-based material having a boride layer. The boriding process was carried out at 850 °C, 950 °C and 1050 °C for 3, 5 and 10 h. The morphology of the boride layer was observed by a metallographic microscope, and the thickness of the boride layer was measured. The surface hardness of the boride layer was measured by a Rockwell hardness tester, the phase composition of the boride layer was analyzed by X-ray diffractometer and the friction and wear properties of the sample were tested on the HT-1000 friction and wear tester. The results show that the boride layer was mainly composed of Fe2B single phase, and its thickness was uniform and firmly bonded to the substrate. The thickness and hardness of the layer gradually increased with time and temperature. The binding force between the layer and the substrate would be decreased while the thickness of the layer was too thin or too thick. Boriding at 850 °C and 950 °C resulted with formation of Fe2B phases, while FeB and Fe2B boride phases occurred at 1050 °C. The boride layer has good wear resistance in the friction and wear experiments, the wear mechanism of the boride specimen is mainly the fatigue spalling caused by plastic deformation of microcracks, while the un-bored samples show severe oxidation and plastic deformation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.