Abstract

In situ laser diffraction, scanning electron microscopy (SEM) imaging, and thermography have been used to investigate particle formation and particle size distribution of alkyl ketene dimer (AKD) produced by rapid expansion of supercritical solution (RESS). The investigated RESS process is based on an earlier reported method to prepare superhydrophobic coatings. Spray distance, pre-expansion temperature and pressure have been varied and the results from the methods have been compared. SEM images and light scattering data correlate well, and show that the mean particle size increased and the size distribution became significantly broader with increasing spray distance. Mean particle diameters of above 5μm were only observed for pre-expansion temperatures at 50°C or below. Furthermore, results show that by placing the surface to be coated within the cold expansion zone of carbon dioxide (CO2), i.e. in this study at 55mm or shorter for a pre-expansion temperature (Tpe) and pressure (Ppe) of 57°C and 180bar, respectively, will produce a surface evenly covered by 3-μm crystalline AKD flake-like particles. Obtained results also indicated, but did not prove, that agglomerates of AKD particles were carried to the surface by liquid CO2 droplets in the jet.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.