Abstract
Strontium–lanthanum–aluminoborosilicate (SrO–La2O3–Al2O3–B2O3–SiO2) (SLABS) glass was prepared for sealant material in planar Solid Oxide Fuel Cells (pSOFC). Differential Thermal Analysis of the glass showed the formation of two crystalline phases, first one 807 °C and the second phase at 1021 °C. Crystallization kinetic of the first crystalline phase was investigated by differential thermal analysis (DTA) and using the JMA-kinetic model. The activation energy for crystallization was calculated to be 114.04 kJ/mol with frequency factor 5.9 × 103. Coefficient of Thermal Expansion (CTE) of the glass was measured to be 9.72 × 10−6/°C. Optical band gap of the glass was measured to be 3.07 eV. Conductivity measured by Impedance spectroscopy found to be 5.68 × 10−7 S cm−1 at 600 °C and it increased with temperature to 2.68 × 10−6 S cm−1 at 800 °C. Activation energy for electrical conduction was measured to be 66.12 kJ/mol. Wetting behavior of the glass on a ferritic steel substrate was investigated under hot stage microscopy. It showed initial deformation temperature (IDT) 754 °C, softening temperature (ST) 840 °C, hemispherical temperature (HT) 1108 °C and flow temperature (FT) 1279 °C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.