Abstract
Purpose The purpose of this paper is to identify the corrosion failure mechanism of a Cu tube in a hydraulic installation and recommend corrective actions to improve the reliability of the entire unit. Design/methodology/approach Failure investigation process includes mainly stereo-, light optical microscopy and scanning electron microscopy as the main analytical tools for material characterization and root-cause analysis. Findings The investigation findings, obtained by corroded surface analysis and metallographic evaluation in transverse sections, suggest strongly that the failure was caused by the operation of Type I pitting corrosion mechanism initiated from the inner side and propagated towards the outer tube surface, assisted by the flowing medium composition. Originality/value This paper deals with an applied failure analysis/case history, summarizes the stages involved in the mechanism of pitting corrosion Type I, taken place in cold water systems together with the main parameters and corrosive species that enhance corrosion rates, shortening pipeline operation life.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.