Abstract

Dimethylol dihydroxyethylene urea (DMDHEU)-treated cotton fabrics were treated with alkali or alternatively acid followed by alkali for increasing time periods, and their effectiveness in removing the crosslinking agent was investigated by surface (X-ray photoelectron spectroscopy) analysis, bulk analysis, crease recovery angle performance and solubility in specific solvents. The cellulose yield after the chemical stripping processes was established and the effect of the acid and alkali treatments on the degree of polymerisation of the resultant cellulose determined. Surface and bulk analyses and solubility tests suggested that alkali alone could not remove the DMDHEU from the crease-resist-treated cotton fabric. However, a sequential acid/alkali treatment effectively removed the easy-care finish from the cotton fabric and produced a commercially viable yield of cellulose.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.