Abstract

ABSTRACT The current study aims in finding the utilization of Industrial waste such as copper and steel slags as a partial replacement material for sand in Sand Compaction Pile (SCP) in proportions of 5%, 10%, 15%, 20%, 30%, and 40% by weight. From the direct shear tests, it is observed that the angle of internal friction increases from 27.59° to 40.1° and 34.82° for copper and steel slags, respectively. The tests are done by installing the SCP in a soft clay in California Bearing Ratio mould and it is tested under soaked and unsoaked conditions. The optimum percentage found from the study for both the slag material is 30%. Tests were also done by air-curing the composite soil within the mould for 7 days and water-curing the sample under soaked conditions for 4 days for the optimum replacement percentage.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.