Abstract

The final product(s) of self‐propagating synthesis are shown to be intrinsically denser than the starting reactants. This behavior results in intrinsic decreases in the sample volume that increase with both the heat of reaction and the adiabatic combustion temperature. Forming of liquid product(s) during reaction simply adds another intrinsic source of porosity, i.e. changes in volume on product solidification. Thus, obtaining fully dense bodies from self‐propagating synthesis requires a mechanism for reducing porosity, e.g. hot‐pressing.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.