Abstract

Three series of dilute iron alloys, with oversized solutes, FeTi, FeV and FeMo, in the concentration range 50 at.ppm to 3 at.%, have been electron-irradiated at low temperature together with the metal. A strong dependence of the solute and defect resistivities on the solute concentration is observed, which is analysed in terms of the two-current model. The specimens have then been annealed throughout stage I (self-interstitial migration) and stage II up to stage III (vacancy migration), with their resistivity measured. In these alloys, the mobile Fe self-interstitials, which are not annihilated at vacancies, are observed to get trapped at solute atoms in stage I and released from traps in stage II. Detrapping occurs in stage I at a temperature, TII, depending on the solute. Trapping is the weakest for V (TII approximately=140 K) and the strongest for Ti (TII approximately=180 K). At very low concentration (50 and 100 at.ppm), the solute trapping efficiency is lost at the beginning of stage III (200 K) for all these solutes. In the most concentrated FeMo alloys, an important fraction of the radiation-induced resistivity is retained at 200 K, due to multiple trapping (trapping of iron interstitials by more than one Mo atom).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.