Abstract

The scanning electron microscope (SEM) and optical microscope (OM) were used to study the deformation of TC18 titanium alloy microstructure at 881°C and 896°C. And the basket weave structure fracture mechanism was discussed. The results have been shown: during deformation at 881°C, the TC18 titanium alloy β grain size of about 305μm and the discontinuous grain boundary α phase along the β grain boundary were obtained. With the deformation temperature rising to 896°C, the β grain growth of 510μm and the continuous grain boundary α phase along the straight β grain boundary were obtained. The TC18 titanium alloy fracture toughness decreased from 77.8 MPa·m1/2 to 65.4 MPa·m1/2 as the rising of deformation temperature from 881°C to 896°C. The average β grain size is about 305μm and the discontinuous grain boundary α phase leads to the higher fracture toughness of TC18 titanium alloy forging. The fracture mode of fine β grain and discontinuous grain boundary α phase is the transgranular fracture, while the coarse β grain and continuous grain boundary α phase is the intergranular fracture.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call