Abstract
Intermetallic tungsten silicide alloy WSi2–W5Si3 was successfully synthesized via magnesiothermic SHS reaction in the WO3–Si–Mg system. Equilibrium composition of combustion products was calculated by standard Gibbs energy minimization method and the combustion products were characterized by XRD, SEM, and EDX. The synthesized alloy had a density of 8.97 g/cm3 (96.4% of theoretical). The process can be readily recommended for practical implementation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Self-Propagating High-Temperature Synthesis
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.