Abstract
Measurements of the capillary length in phase-separated solutions of polymethylmethacrylate in 3-octanone (PMMA/3-OCT) for each of five different molecular weights of PMMA, and in phase-separated solutions of polystyrene in methylcyclohexane (PS/MCH) for a single molecular weight of polymer, are reported. Measurements on PMMA/3-OCT were by the sessile-drop method; those on PS/MCH were by both the sessile-drop and capillary-rise methods. Interfacial tensions are estimated from estimated density differences and the measured capillary lengths. A theoretically predicted scaling law for the dependence of capillary length on polymer molecular weight and temperature is tested and at least semiquantitatively verified. As by-products of the sample preparation, the molecular-weight dependences of the critical composition and critical solution temperature of PMMA/3-OCT were also determined. The volume fraction of polymer at the critical point, φc, is found to be proportional to the −0.37±0.01 power of the molecular weight, in agreement with values of this exponent found by others for polystyrene solutions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.