AbstractSulfide‐based all‐solid‐state battery (ASSB) with a lithium metal anode (LMA) is a promising candidate to surpass conventional Li‐ion batteries owing to their inherent safety against fire hazards and potential to achieve a higher energy density. However, the narrow electrochemical stability window and chemical reactivity of the sulfide solid electrolyte towards the LMA results in interfacial degradation and poor electrochemical performance. In this direction, we introduce an organic additive approach, that is the mixing of prelithiated trithiocyanuric acid, Li3TCA, with Li6PS5Cl, to establish a stable interface while preserving high ionic conductivity. Including 2.5 wt % Li3TCA alleviates the decomposition of the electrolyte on the lithium metal interface, decreasing the Li2S content in the solid‐electrolyte interface (SEI) thus forming a more stable interface. In Li|Li symmetric cells, this strategy enables a rise in the critical current density from 1.0 to 1.9 mA cm−2 and stable cycling for over 750 hours at a high current density of 1.0 mA cm−2. This approach also enables Li|NbO‐NCM811 full cell to operate more than 500 cycles at 0.3 C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.