Abstract
In order to extend the use of a SiO2–Al2O3–ZnO–CaO based glass coating for higher temperature applications on Ni-base superalloy substrates, its interfacial reaction with the K38G superalloy substrates at 1000°C was investigated. Results indicated that the interfacial reaction resulted in bubbling of the glass coatings due to Zn gas volatilization and formation of a loose TiO2 interlayer which finally accounted for the peeling of the coatings. With a pre-crystallization process of the glasses, its interfacial reaction was controlled and the bubbling of the coatings was avoided. After the heat-treatment at 1000°C for 20h, the glass coatings were still very dense and bonded well to the K38G superalloy substrates. Instead of a loose TiO2 interlayer, an Al-riched layer formed at the interfaces.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.