Abstract

Bimetallic castings are widely employed as working elements in winning machines which work in conditions of intensive friction wear. The main features of wear are: dynamic percussive loads, intensive abrasive wear caused by erosion and corrosion. Three cylindrical rods cavities of the same dimensions of φ 20x200 mm were made in sand mould. Different amount of liquid iron alloy with carbon equivalent of 4.14, Mn of 0.58 and Cu of 0.17 wt% was poured into the three rod cylindrical cavities over the solid 304 stainless steels cylindrical desks inserts. Good coherent interfaces for all liquid/Solid volumes (16 to 24) are produced and multi-layers interfacial microstructure bimetal are produced. Increasing the liquid/solid volumes from 16 to 24 increases the thickness of transient layer from 52 to 89 μm and decreases the amount of ledeburite in the structure of solidified gray cast iron.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.