Abstract

We report a promising method for oxide-layer-free germanium (Ge)/silicon (Si) wafer bonding based on an amorphous Ge (a-Ge) intermediate layer between Si and Ge wafers. The effect of the exposure time (te), during which the a-Ge is exposed to the air after sputtering and being taken out of the chamber on the bubble density at the bonded interface, is identified and a near-bubble-free Ge/Si bonded interface is achieved for the te of 3 s. The crystallization of a-Ge at Ge/Si bonded interface starts from a-Ge/Ge interface and it fully turns to be single-crystal Ge after post-annealing. The oxide layer at a-Ge/a-Ge bonded interface formed by the interface hydrophilic reaction disappears due to the atom redistribution triggered by the crystallization of a-Ge. As expected, the performance of the Ge/Si heterojunction diode is significantly improved by this oxide-layer-free Ge/Si bonded interface. A low dark current of 1.6 µA, high on/off current ratio of 3.4 × 105, and low ideality factor of 1.02 (150 K) is achieved at −0.5 V for the bonded Ge/Si diode. Finally, the carrier transport mechanisms at Ge/Si bonded interface annealed at different temperatures are also clearly clarified.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.