In this work we study brazing of Al2O3 to Ti with biocompatibility properties, using a Au-foil as joining element. Al2O3 was produced by sintering of powder at 1550°C. Al2O3 samples were coated with a 2 and 4μm thick of Mo layer and then stacked with Ti. Al2O3–Mo/Au/Ti combinations were joined at 1100°C in vacuum. Successful joining of Mo–Al2O3 to Ti was observed. Interface shows the formation of a homogeneous diffusion zone. Mo diffused inside Au forming a concentration line. Ti3Au and TiAu phases were observed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.