Abstract

physica status solidi (b)Volume 22, Issue 2 p. K71-K74 Short Note Interaction of Dislocations with Coherent Particles and Stress Corrosion Cracking of High-Strength Aluminum Alloys M. O. Speidel, M. O. Speidel Boeing Scientific Research Laboratories, Seattle, WashingtonSearch for more papers by this author M. O. Speidel, M. O. Speidel Boeing Scientific Research Laboratories, Seattle, WashingtonSearch for more papers by this author First published: 1967 https://doi.org/10.1002/pssb.19670220246Citations: 11AboutPDF ToolsRequest permissionExport citationAdd to favoritesTrack citation ShareShare Give accessShare full text accessShare full-text accessPlease review our Terms and Conditions of Use and check box below to share full-text version of article.I have read and accept the Wiley Online Library Terms and Conditions of UseShareable LinkUse the link below to share a full-text version of this article with your friends and colleagues. Learn more.Copy URL Share a linkShare onFacebookTwitterLinked InRedditWechat Citing Literature Volume22, Issue21967Pages K71-K74 RelatedInformation

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.