Abstract

The hydrothermal reduction of cobalt and manganese nitrates with graphite in the temperature range of 250-3500C has been investigated to obtain nanosized spinel structures. As a result, Co2Mn3O8 and (Co,Mn)(Co,Mn)2O4 spinel phases with average particle sizes of 42 nm and 66 nm have been obtained depending upon reaction conditions (temperature, reaction time and ratio of reagents). The compounds had the following compositions in accordance with the data of energy dispersive analysis (EDA): C-graphite - 86.2%, Co2Mn3O8 - 13.8%, and C-graphite - 93.2%; (Co,Mn)(Co,Mn)2O4 - 4.8%, Mn3O4 - 1.6%, Co3O4 - 0.5%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.