Silicon offers high theoretical capacity as a negative electrode material for lithium-ion batteries; however, high irreversible capacity upon initial cycling and poor cycle life have limited commercial adoption. In this work, an operando isothermal microcalorimetry (IMC) study of a model system containing lithium metal and silicon composite film electrodes was reported on the first two cycles of (de)lithiation. The total heat flow data are analyzed in terms of polarization, entropic, and parasitic heat flow contributions to quantify and determine the onset of parasitic reactions. These parasitic reactions, which include solid−electrolyte interphase formation, contribute to electrochemical irreversibility. To complement the calorimetry, operando X-ray diffraction is used to track the phase evolution of silicon. During cycle 1 lithiation, crystalline Si undergoes transformation to amorphous lithiated silicon and ultimately to crystalline Li15Si4. The solid-state amorphization process is correlated to a decrease in entropic heat flow, suggesting that heat associated with the amorphization contributes significantly to the entropic heat flow term. This study effectively uses IMC to probe the parasitic reactions that occur during lithiation of a silicon electrode, demonstrating an approach that can be broadly applied to quantify parasitic reactions in other complex systems.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.