Natural rubber (NR) and halloysite nanotube (HNT) composites are known to perform poorly due to polarity differences between the two components. As such, many extant studies have attempted to increase their compatibility. Therefore, this study introduced epoxidized natural rubber (ENR) together with silane coupling agents into the composite to ensure rubber-filler interactions. Four different silanes namely bis-[(triethoxysilyl)propyl] disulphide (TESPD), bis[(triethoxysilyl)propyl] tetrasulfide (TESPT), triethoxyvinylsilane (VTEO), and 3-mercaptopropyl-di(tridecan-1-oxy-13-penta(ethyleneoxide)) ethoxysilane (VPSi-363) were used. Fourier-transform infrared (FTIR) spectroscopy of the composite confirmed the formation of hydrogen bonds between the silane as the peak of Si-O shifted to higher wavenumbers; i.e., 1080 cm-1 to 1042 cm-1. Silane was also found to improve the tensile strength, modulus and tear strength regardless of functionality. This was further supported by the findings of the Payne effect. As for strain-induced crystallisation (SIC), the stress-strain curves agreed well with the development of crystallinity observed during synchrotron wide-angle X-ray scattering analysis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.