Abstract
In-line optical fiber polarizer and modulator were fabricated by depositing Langmuir-Blodgett (LB) films on polished fiber surface with gold layer. The thickness of LB film was adjusted by changing the number of monolayers, which then optimized the performance of the fiber polarizer. Good agreement was observed between the theoretically predicted conditions for efficient coupling and the experimentally determined conditions for high TM/TE extinction ratio of the optical field. By applying an electric field between the LB film, the polarization state of the lightwave in the optical fiber can be modulated.< <ETX xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">></ETX>
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.