Abstract

Based on a previous optimisation of set-up parameters for injection moulding of polyamide 6-6 (PA 6-6) rein- forced with 40 wt% of 10 mm long glass fibre, the aim of this paper is to define suitable guidelines to further improve the mechanical performances of PA 6-6/glass long fibre thermoplastic (LFT) injection mouldings. Different solutions have been considered: screw and non-return valve design modification so as to adapt them to LFT processing, increase of the ini- tial fibre content (up to 50 wt%) and length (up to 25 mm) in the LFT pellets. Using a LFT dedicated plasticating unit has allowed decreasing the fibre breakage amount by about 80% at the nozzle exit, however without improving the flexural properties. Increasing the initial fibre content has logically permitted to improve the flexural properties. Increasing the ini- tial fibre length has not brought any improvement of the properties and has even amplified the structural heterogeneities and anisotropy of the parts. These trends have been explained on the basis of cavity pressure records highlighting signifi- cantly different rheological behaviours, and of resulting residual fibre lengths and through-the-thickness fibre orientation profiles modifications.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.