Abstract

BackgroundsThe purpose of this study was to quantify the initial stability of a highly porous titanium cup using an acetabular bone defect model. MethodsThe maximum torque of a highly porous titanium cup, with a pore size of 640 μm and porosity of 60%, was measured using rotational and lever-out torque testing and compared to that of a titanium-sprayed cup. The bone models were prepared using a polyurethane foam block and had three levels of bone coverage: 100, 70, and 50%. ResultsThe highly porous titanium cup demonstrated significantly higher maximum torque than the titanium-sprayed cups in the three levels of bone defects. On rotational torque testing, it was found to be 1.5, 1.3, and 1.3 times stronger than the titanium-sprayed cups with 100, 70 and 50% bone coverage, respectively. Furthermore, it was found to be 2.2, 2.3, and 1.5 times stronger on lever-out testing than the titanium-sprayed cup. No breakage in the porous layers was noted during the testing. ConclusionThis study provides additional evidence of the initial stability of highly porous titanium cup, even in the presence of acetabular bone defects.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.