Abstract

In order to confirm the formation of a tungsten fiberform nanostructure (W-fuzz) by helium plasma exposure in the large-sized plasma confinement device, the bulk tungsten with the size of 80 × 20 × 1.5 mm3 was inserted into the divertor leg position in the Large Helical Device (LHD). Then, it was exposed to the divertor plasma during the ultra-long pulse helium discharges with 10,190s in total. The width of the divertor plasma, incident ion energy and total fluence were expected to be ∼2cm, 100–200eV and ∼5 ×1025 He/m2 (strike position), respectively. The surface temperature of the tungsten specimen was monitored by IR camera. The typical surface temperature of the divertor strike point was estimated to be around 1900∼2300K. After the exposure, an initial growth phase of tungsten fiberform nanostructure (W-fuzz) was able to be identified on the tungsten surface. The finest initial growth phase of the W-fuzz structure was able to be identified on the central region of the divertor strike point, where retention amount of helium was estimated to be ∼8 ×1021 He/m2. This study is the first simultaneous evaluation of the W-fuzz growth and quantification of the helium retention in the large-sized plasma confinement device.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call