Friction stir processing (FSP) has demonstrated to refine the microstructure of different alloys resulting in superior mechanical properties. Abnormal grain growth (AGG) has been recognized as a critical issue during hot deformation of FSPed Al alloys. 5083 Al alloys with different Mn content were subjected to heat treatments at 350 and 535°C before FSP to avoid AGG during subsequent hot deformation. As a result, heat treatment of 350°C was able to retard AGG significantly. Also, an improvement in the refinement of the microstructure was observed. Consequently, a better ductility of 861% at elevated temperature was reached in the alloy with lower Mn content comparing with the same alloy without heat treatment prior to FSP.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.