Abstract
This work demonstrates area-selective growth of tungsten (W) films by hot-wire assisted atomic layer deposition (HWALD). With this recently developed technique, low-resistivity alpha-phase W films can be deposited by using sequential pulses of atomic hydrogen (at-H) and WF6 at a substrate temperature of 275 °C. As reported in this article, the deposition is highly selective. HWALD tungsten grows with little to no incubation time on W, Co and Si surfaces. On the other hand, no growth is observed on TiN, Al2O3 and SiO2 surfaces. The interfaces of W and various substrates are examined by transmission electron microscopy. The absence of oxygen in the interfaces indicates that the atomic-hydrogen not only serves as a suitable ALD precursor for W, but is here shown to effectively reduce the native oxides of W and Co at the ALD process conditions, enabling in situ surface preparation before starting the deposition sequence.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.