nfluencing factors of target products such as X phase, β-SiAlON phase and O-SiAlON phase of Inner Mongolia coal gangue carbothermal reduction and nitridation were researched by calculating the loss rate on ignition of specimens, and by means of XRD and SEM. During the carbothermal reduction and nitridation reaction of coal gangue, the loss rate on ignition of specimens rises with carbon reducer increasing, and keeping time has a little influence on the loss rate on ignition of specimens. If β-SiAlON is target phase, the yield from corundum is much higher than that from special grade bauxite. Corundum or bauxite is used as starting material, the yield of X phase is low and the highest yield is only 12.88%. For the carbothermal reduction and nitridation reaction of coal gangue, the appropriate addition of reducer carbon is 10%-16%, and temperature influence is larger. The reaction temperature over 1420°C and keeping time of 6h are beneficial to the formation of X phase, β-SiAlON and O-SiAlON.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.