Abstract

This work aims to study the effect of radiolytic species induced by water radiolysis on the passive behavior of 316L stainless steel. For this purpose, the stainless steel/neutral and aerated 0.02 M Na2SO4, electrolyte solution interface was irradiated with proton beams. A wide range of energies between 2 and 16 MeV was selected, varying the maximum of the energy deposition between 0.5 and 122 μm in water from the interface. The irradiation experiments were performed at the CEMHTI cyclotron in Orléans and the 4 MV Van de Graaff accelerator at IP2I in Lyon (France). A dedicated irradiation device implemented with a 3-electrode cell dedicated to perform electrochemical measurements allows to measure the surface reactivity of the stainless steel as a function of the irradiation conditions. Results show that whatever the beam energy, the corrosion potential remains unchanged. It indicates that the very short-lived, highly reactive radiolytic species drive the corrosion potential and not only the recombination products such H2O2 or H2. The stainless steel remains in the passive state whatever the irradiation conditions. However, it is shown that, during irradiation, the passive film is less protective. This evolution is attributed to radiolysis of bound water molecules in the passive film.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.