Abstract
The present work investigates the performance of TiAlSiVN coating with 5 and 11 at% of V concentration deposited on the Al2O3/SiC cutting tools during dry turning of austenitic 316 L stainless steel. The maximum flank wear reduction compared to the uncoated tool for coated tools with 11% and 5% V concentration was 85% and 67%, respectively. The Raman analysis indicated the formation of V2O5 in the cutting zone, which helps to reduce friction and machining forces for the coated tools. Overall, the presence of higher V content (11 at%) enhances the self-lubrication behaviour of the TiAlSiVN coating, accounting to lower fluctuations in cutting forces, superior surface finish, and lower flank wear when compared to the TiAlSiV5N coated and uncoated cutting tools.
Published Version (Free)
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.