Abstract

The experimental results for manufacturing ceramics from industrial boron carbide powder with 10 wt% of ultradispersed fraction of a powder of the same composition by spark plasma sintering have been presented. Under optimal process conditions such sintering results in a decrease of the sintering temperature and synthesis time, and the addition of ultradispersed fraction increases microhardness and fracture toughness of the ceramics.