Abstract
AbstractThe safety‐critical rotating parts of aircraft engines are mainly designed using experimental material data, based on standard specimens and procedures, while few data are available on the effect of manufacturing anomalies on fatigue life. In this context, the paper investigates the effects of different machining parameters on the high‐temperature fatigue resistance of Inconel 718 superalloy specimens, cut from engine disk forgings, machined by turning on a vertical lathe. An unconventional specimen was designed in order to have the machining marks aligned with the fatigue loading axis, so to reproduce the hoop stresses in engine disks. For the test campaign, three machining parameters were chosen (depth of cut, cutting speed and insert wear) that typically may generate non‐geometrical anomalies. A correlation has been found between the machining parameters, the residual stresses, the surface roughness, and the distorted and amorphous layer thicknesses. Correlations of such data with fatigue life are also presented and discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Fatigue & Fracture of Engineering Materials & Structures
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.