Abstract
In this study, the impact of different tool geometries on the limiting drawing ratio (LDR) in micro deep drawing was investigated. Experimental micro deep drawing tests to determine the limiting drawing ratios were carried out for a variation of the punch diameter, the die radius and the die clearance. In order to assess the impact of the material properties on the process limits the foil materials Al99.5 and E-Cu58, both with a thickness of 20 μm, and the stainless austenitic nickel-chromium steel 1.4301 (X5CrNi18-10) with a thickness of 25 μm were investigated. The results reveal an increase of the limiting drawing ratio with increasing die radius size for the foil materials E-Cu58 and austenitic steel. For a decrease of the die clearance to values smaller than 1.25 times the foil thickness an increase of the limiting drawing ratio was determined for all three materials.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.