The influence of Cr2O3, TiO2 and ZrO2 on the sintering, crystallisation and machinability of SiO2–Al2O3–MgO–K2O–B2O3–F glasses was investigated. Optimum fluoromica glass ceramic compositions with desirable sintering behaviour and machinability were obtained by addition of titanium and chromium oxides to the base glass. Texture and relative intensity of mica phase Imica/ISi were determined by XRD analysis and the particle size distribution of chips was studied by drilling. Microhardness and bending strength were also investigated. The relative intensity of mica phase and microhardness were found to be compatible with the experimental results.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.