This paper deals with the wear and mechanical (tensile, compressive, and microhardness) properties of Mg/TiC composites over magnesium alloy (AZ91D). Magnesium based metal matrix (AZ91D) composites were synthesized by using TiC particles varying wt % from 0% to 20% with a step of 5% by stir casting. The mechanical properties shows there is significant improvement of ultimate tensile strength (UTS) & % elongation, compressive strength, and microhardness with % increase of TiC content in Mg alloy. The fracture mechanism of the tensile and compressive specimen was investigated by Scanning Electron Microscope (SEM). A Pin-on-Disk (POD) tribotester was used to determine the wear rate (WR) and specific wear rate (SWR) of the composites. The test was carried out in a dry sliding condition of varying load of 10N, 30N and 50 N corresponding to a constant sliding distance & sliding speed of 1000 m and 1 m/s respectively and the worn surface of the pin is examined by SEM after the test.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.