Abstract

Al-12Si-3.2Cu-1Mg-2.4Ni-χTi (χ=0, 0.2) alloys were prepared by squeeze casting process, and then heat-treated. The mechanical properties were tested at 350°C, the microstructure and phases in them were investigated by optical microscope, SEM, EDS and XRD. It is found that the grain size has an obvious increment after 0.2 wt. % Ti additions to Al-12Si-3.2Cu-1Mg-2.4Ni, and the ultimate tensile strength at elevated-temperature increased accordingly. Intermetallic compounds, such as γ-Al7Cu4Ni, M-Mg2Si, Q-Al5Cu2Mg8Si6 and δ-Al3CuNi existing in alloys with and without Ti addition. Needle-like Ti containing phase with the elements of Al, Si and Ti created in Al-12Si-3.2Cu-1Mg-2.4Ni-0.2Ti alloy, and the eutectic Si is found to distribute by the side of Ti containing phase.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.