Abstract

The present paper investigates the influence of thermo-vacuum treatment at 170, 190 and 210 °C on the mechanical and physical properties of poplar wood rotary-cut veneers obtained from two different poplar clones (’I-214’ and ’Lena’). The modulus of rupture in bending was determined according to a method derived from European Standard EN-310 and previously validated by the authors, while the density was determined on the basis of EN-323. With both clones no significant decrease was recorded either in bending strength or in density with treatment temperatures up to 190 °C. On the contrary, at 210 °C a highly significant decrease in modulus of rupture (’I-214’: -18%; ’Lena’: -15%) was recorded; the density showed a similar, though lower, trend (’I-214’: -5 %; ’Lena’: -8.5 %).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.