Abstract
The purpose of this study was to verify for various glass-ionomer cement (GIC) products whether the application of thermo-light curing on the initial curing material produces an increase in microhardness, and to determine whether this hardness varies depending on the depths of the GIC samples. The efficacy of various polymerization units on this additional hardening was also examined. The GIC samples were thermo-light cured for 60 seconds with three polymerization units. The Vickers microhardness was measured at three different depths: 2 mm, 3 mm, and 4 mm. Analysis of variance and Newman-Keuls test showed statistically significant differences among tested samples for all three GIC groups (P < .001). The results of linear regression analysis showed a statistically significant relationship between the hardness of the material and the temperature for samples with depths of 2 mm (R = 0.78; P = .0028) and 3 mm (R = 0.59; P = .045). The findings of this study indicate that thermo-light curing of GIC with different polymerization units for 60 seconds during setting reaction increases the microhardness of the GICs at all depths tested and may increase resistance to mastication forces, which can be validated in future clinical studies.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: The International Journal of Periodontics & Restorative Dentistry
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.