Abstract
It has been shown that the thermal fixation of the fibre with hot air at 195°C leads to the optimum results. Under these conditions the highest light-fastness of the triacetate fibre is achieved, the tensile strength and elongation at break do not decrease so markedly, and practically no chemical changes take place.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.