Abstract

The formation of surface defects on 125 × 125 and 150 × 150 mm billet rolled in the reduction shop is considered. The influence of rolling and straightening on the product quality is studied. The proposed approach permits timely corrective and preventive measures to increase the billet yield.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.