Abstract

Silk fibroin (SF) was regenerated using three of the most common protocols described in the bibliography for the dissolution of raw SF (LiBr 9.3M, CaCl2 50wt.% or CaCl2:EtOH:H2O 1:2:8 in molar ratio). The integrity of regenerated SF in aqueous solution was analyzed by SDS-PAGE and different profiles of degradation were observed depending on the protocol used. This fact was found to affect also the aqueous solubility of the freeze dried protein. These different SFs were used to produce electrospun mats using SF solutions of SF 17wt.% in 1,1,1,1′,1′,1′-hexafluoro-2-propanol (HFIP) and significant differences in fiber sizes, elongation and ultimate strength values were found. This work provides a global overview of the manner that different methods of SF extraction can affect the properties of electrospun SF-mats and consequently it should be considered depending on the use they are going to be made for.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.