Abstract
This paper covers gold leaching from sulfide ores. The data on the silicate, mineral, and grain-size composition are presented for the ore studied. Agitation leaching studies were completed for the combined sample and direct cyanidation dynamics indicators are established for the material sample. For all material with the grain size class of 95 % passing –0.074 mm, the required agitation leaching duration is 9–10 hours; with the material sizes up to 2 mm, the leaching duration shall be at least 22 hours. In order to study the efficiency of using roller presses as an alternative to fine crushing, two percolation leaching tests were conducted for the ore size of –5 mm. The material for the first test was prepared by crushing in a standard jaw crusher and the material for the second test was prepared by crushing in a laboratory press with complex monolayer reduction. It has been found that ore reduction using high-pressure crushers, as compared to standard crushing equipment, allows increasing gold recovery during subsequent leaching by 13.52 %. At the same time, the consumption of sodium cyanide increases by 0.26 kg/t of ore.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.