Abstract
CO–O2 kinetics was studied on Rh(0.3 wt%)/SnO2 and compared with that reported previously on Rh/Ce0.68Zr0.32O2. The lower oxygen mobility on SnO2 and the stronger bonding of CO with the Rhδ+ sites of Rh/SnO2, are suggested to account for the lower CO oxidation activity of Rh/SnO2 compared with that reported on Rh/Ce0.68Zr0.32O2.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.