Abstract

The lateral use of the laser in laser-assisted WAAM processes, resulting in a directional dependence, can influence the bead shape and the bead surface. The influence of the laser position on the weld bead is investigated. Beads with different laser positions are applied and the height and width as well as the waviness of the beads are evaluated. In addition, claddings are welded and the waviness is measured. The waviness along the beads ranges from 8.77 to 34.66 µm, and no significant correlation with the welding direction could be determined. For the bead shape, the differences in height range from 3.54 to 3.90 mm and in width from 8.20 to 8.89 mm. Based on the results, a dependence on the laser position for surface properties and weld bead shape becomes clear.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.