Abstract

Y and Nd are simultaneously added into Mg–5Li–3Al–2Zn alloy. It is found that there exist the phases of α-Mg, AlLi, Al11Nd3 and Al2Y in the alloys. When the contents of Y and Nd are 1.2% and 0.8%, respectively, the grain is the finest with an average size of 30μm, and the tensile strength of the alloy reaches 231MPa, the elongation reaches 16%. When the ratio of Y to Nd is 1.2:0.8, there is a synergistic strengthening effect.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.