Abstract

The dependences of the maximal first order diffraction efficiency and the corresponding specific recording energy on the holographic grating period were studied. Grating period was varied from 0.40 to 70.0 μm. Both fresh and aged films were used. A large holographic recording efficiency decrease in the course of aging is found to take place. These changes are due to the effective film grain size increase caused by the relaxational structural changes and atmospheric oxygen exposure. Results are explained with the aid of stress fields induced by the evaporation and holographic recording. The obtained results can be used to optimize the hologram recording in amorphous chalcogenide films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.