Abstract
Abstract Surface treatments usually are used to modify the appearance and properties of stainless steel surfaces. Simultaneously, the corrosion resistance of the stainless steel surface being related intrinsically to the spontaneous formation of a passive layer also will be affected. In this respect, the influence of different surface treatments on the corrosion resistance of Type 304 (UNS S30400) stainless steel to pitting corrosion has been evaluated by means of potentiostatic electrochemical noise measurements and surface characterization. Typical industrial treatments including mechanical grinding, glass blasting, and pickling were taken into account. Additionally, special consideration was put on the effect of aging conditions of the passive layer after surface treatments, in particular on the relative humidity. Benefits and limitations of the different applied surface treatments concerning protectiveness of the stainless steel surface were determined and discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have